System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
MetalTek C86300 High Tensile Manganese Bronze
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
;
Bronze
Material Notes:
High strength and hardness copper-zinc alloy.
Applications: Steel mill nuts, ordnance parts, worm gears.
Information provided by MetalTek
Cast UNS C86300; Cast Grade C86300; Cast ASTM B271, B584, B148; Military MIL-C-15345-6; SAE 430B (Discontinued)
Key Words:
Yellow Brass
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Original Value
Comments
Hardness, Brinell
229
Tensile Strength, Ultimate
>=
760
MPa
Tensile Strength, Yield
>=
415
MPa
Elongation at Break
>= 12 %
Component Elements Properties
Original Value
Comments
Aluminum, Al
6.0 %
Copper, Cu
63 %
Iron, Fe
3.0 %
Manganese, Mn
3.0 %
Zinc, Zn
25 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Manganese Bronze, UNS C86300, Copper Casting Alloy
MetalTek MTEK 175-C Cast UNS C95400HT Aluminum Bronze
MetalTek C86200 Med. Tensile Manganese Bronze
Manganese Bronze, UNS C86200, Copper Casting Alloy
Manganese Bronze A, UNS C67500
NMETEK035 / 18285
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.