MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 10042 Polypropylene, Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA Polypropylene PPH 10042 is a nucleated antistatic homopolymer. PPH 10042 is characterized by high fluidity for high speed injection of thin wall articles such as dairy pots and tubs, salad trays and caps and closures.

Application

PPH 10042 is nucleated and thus has improved rigidity. This coupled with a highly antistatic nature allows for shorter cycle times and easy demolding.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.525 g/ccISO 1183
Density 0.905 g/ccISO 1183
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ISO 2039-2
Tensile Strength, Yield 35.0 MPaISO 527-2
Elongation at Yield 8.5 %ISO 527-2
Tensile Modulus 1.70 GPaISO 527-2
Flexural Modulus 1.60 GPaISO 527-2
Izod Impact, Notched (ISO) 3.00 kJ/m²ISO 179
Charpy Impact, Notched 0.350 J/cm²ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 105 °C120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C120°C per hour; ISO 75-2
Vicat Softening Point 90.0 °C50N-50°C per hour; ISO 306
 153 °C10N-50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® DP 9370A Polyurethane
Ineos L12Z-01 Polypropylene Impact Copolymer
Ineos H19G-01 Polypropylene Homopolymer
Flint Hills P4C6B-134A Polypropylene Homopolymer
Borealis HJ320MO Polypropylene

PFINAA140 / 38576

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.