MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weight distribution and high density combine successfully to give excellent extrudability with high impact properties.

Typical Applications: FI0644 is recommended for blown film extrusion. It can be used for producing heavy duty bags, grocery sacks, shopping bags, refuse bags, liners for multi-wall sacks. The grade is suitable to blend with LLDPE & LDPE and can be used in co-extrusion process.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.944 g/ccISO 1183
Thickness 20.0 microns
Melt Flow 0.18 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 5.4 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ISO 868
Film Tensile Strength at Yield, MD 50.0 MPaISO 527
Film Tensile Strength at Yield, TD 45.0 MPaISO 527
Film Elongation at Break, MD 400 %ISO 527
Film Elongation at Break, TD 450 %ISO 527
Elmendorf Tear Strength MD 20 gISO 6383-2
Elmendorf Tear Strength TD 40 gISO 6383-2
Elmendorf Tear Strength, MD 1.00 g/micronISO 6383-2
Elmendorf Tear Strength, TD 2.00 g/micronISO 6383-2
Dart Drop 13.0 g/micronF50; ASTM D1709
Dart Drop Test 260 gF50; ASTM D1709
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 73.0 °CISO 306
Brittleness Temperature <= -80.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 225 °C
Blow-up Ratio (BUR) 3.0 - 5.0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SABIC 6821N Linear Low Density Polyethylene for Blown Film
SABIC HP0722N Low Density Polyethylene for Blown Film
SABIC F00952EQ High Density Polyethylene for Blown Film
SABIC HP4023W Low Density Polyethylene for Blown Film
SABIC 318CN Linear Low Density Polyethylene for Wire & Cable

PSABICZ801 / 132997

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.