MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® NRG 2101 PA 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: VESTAMID® NRG 2101 yellow is a high molecular grade PA 12 material developed by Evonik. Its superior performance characteristics make it an ideal choice for expanding the use of thermoplastic piping systems at higher operating pressure and larger diameters to replace metallic piping systems in a safe and cost effective manner. Besides extending the operating pressure limits of thermoplastic piping systems, VESTAMID® NRG 2101 yellow offers many of the same benefits, and in most instances more superior performance, as conventional PE piping systems.
  • Tough and durable
  • Corrosion resistant
  • Resistant to heavy hydrocarbons
  • High resistance to Slow Crack Growth and Rapid Crack Propagation
  • Increased installation efficiencies
These characteristics make the VESTAMID® PA12 material an ideal choice when selecting appropriate thermoplastic piping materials in extending gas distribution infrastructure. Manufacturer recommends a processing temperature between 230°C (446°F) and 260°C (500°F) - in some cases up to 280°C (536°F) – during the injection molding and extrusion process. The mold temperature should be within a range of 60°C (140°F) to 100°C (212°F). Drying at 80°C (176°F) for 2 hours to 4 hours before processing is recommended. Polyamide 12 is a high performance thermo plastic polymer with increased performance characteristics that translates into safe operations over the life of the installed pipeline. It has a considerable record of safe and proven experience in many demanding applications, including fuel lines in passenger cars, air brake tubing in trucks and off-shore applications.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73ISO 868
Ball Indentation Hardness 76.0 MPaISO 2039-1
Tensile Strength, Yield 40.0 MPaISO 527
Elongation at Break >= 150 %ISO 527
Elongation at Yield 12 %ISO 527
Tensile Modulus 1350 MPaISO 527
Charpy Impact Unnotched NB
@Temperature -40.0 °C
ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 177 °CISO 11357
Vicat Softening Point 170 °C
@Load 1.02 kg
Method A; ISO 306
 
Descriptive Properties
ColorYellow

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAMID® NRG 1001 PA 12
Evonik VESTAMID® NRG 2901 PA 12
Arkema Pebax® 5533 SA 01 MED Polyether Block Amide (PEBA)
Evonik VESTAMID® NRG 3001 PA 12
Evonik VESTOSINT® 2178 white Polyamide 12

PEVONIL269 / 196473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.