MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Flex® TEA 1004 TPO Thermoplastic Polyolefin Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Features:

  • Adhesion, Good
  • Paintable
  • Weather Resistance, Good
  • Forms:

  • Pellets
  • Uses:

  • Automotive Applications
  • Seals
  • Toothbrush Handles
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.02 g/ccASTM 792
    Linear Mold Shrinkage 0.010 cm/cmASTM D955
    Melt Flow 10 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Ultimate 1530 psiASTM D638
    Elongation at Break 600 %ASTM D638
    Flexural Modulus 3000 psiSecant; ASTM D790
    Izod Impact, Notched NBASTM D256
    Tear Strength 210 pliASTM D624
     
    Thermal PropertiesOriginal ValueComments
    Brittleness Temperature -60.0 °CASTM D746
    Flame Spread <= 0.50 in/minFM VSS-302

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    RTP Company Permaprene™ 2800 B-85A Thermoplastic Polyolefin Elastomer (TEO)
    Multibase Multi-Flex® TEA 4001-35 Natural TPO Thermoplastic Polyolefin Elastomer
    Multibase Multi-Flex® 1047 Black TPO Thermoplastic Polyolefin Elastomer
    Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer
    Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer

    PMULTI115 / 54019

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.