Description: Rulon® films offer superior abrasion resistance when compared to conventional PTFE films. Service temperatures range from -100°F to 500°F (-73°C to +260°C). In rotating bearing tests, it provided a 500-fold increase in wear resistance over standard PTFE. Applications include bearing liners, chute and guide rail coverings. This tape uses a silicone adhesive system. Perfect for extreme temperature applications, silicone adhesives perform in continuous operating temperatures from -100°F to 500° (-73°C to 260°C). Silicone-based adhesive systems exhibit good chemical resistance, retain electrical properties, and remove cleanly with little or no residue. All data based on a 0.01 inch test sample.(Thickness given is for both backing and adhesive. Backing thickness is .008 inches.) Information provided by Saint Gobain Performance Products. |