MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cabot BLACK PEARLS® E Specialty carbon black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: BLACK PEARLS E specialty carbon black is a low structure specialty black pigment suitable for use in UV cure ink applications.

Key applications: BLACK PEARLS E specialty carbon black designed for use in UV ink applications. It is a blue tone pigment black. Due to its oxidized surface, BLACK PEARLS E specialty carbon black disperses well and can impart low viscosity and good dispersion stability. In comparison to other carbon blacks for ink applications, BLACK PEARLS E has lower cure energy and photo initiator requirements. The dispersibility of BLACK PEARLS E specialty carbon black depends on the equipment used and the formulation. A product with similar morphology, MOGUL® E specialty carbon black, is available in an easier-to-disperse fluffy form.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 2.0 %2.0 %CTM 16.1
Particle Mesh Size 325 Mesh325 Mesh<100 ppm; ASTM D-3265
 
Descriptive Properties
Iodine absorption57 mg/gDevolatilized, CTM 23.4
OAN48 cc/100gASTM D-2414
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT028 / 315763

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.