MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Adstif HA622M PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Adstif HA622M is a high crystallinity medium fluidity polypropylene homopolymer. It does not contain slip or antiblocking additives and it does not contain Calcium Stearate. It is nucleated. Adstif HA622M is typically used by customers for cast film applications where high rigidity and high temperature resistance are required. Adstif HA622M is used by customers for the production of coextruded twist wrapping, labels, lamination, metallize able film and textile packaging. Films produced with Adstif HA622M have been reported by customers to exhibits very high stiffness and thermal stability.

Availability: Africa-Middle East; Europe

Application: Barrier Film; Food Packaging Film; Specialty Film; Stationery Film; Twist Wrap Film

Market: Flexible Packaging

Processing Method: Cast Film; Double Bubble

Attribute: Broad Molecular Weight Distribution; Crystalline; High Heat Resistance; High Rigidity; High Stiffness; Homopolymer

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-1
Melt Flow 7.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 28.0 MPaISO 527-1, -2
Tensile Strength, Yield 40.0 MPaISO 527-1, -2
Elongation at Yield 7.00 %ASTM D638
Flexural Modulus 220 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °CUnannealed; ISO 75B-1, -2
Vicat Softening Point 160 °CB/10 N; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9015 / 323943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.