MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3Z HP PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Ultramid A3Z HP is an unfilled, impact modified, heat stabilized, high flow PA66 injection molding grade. Ultramid A3Z HP offers a unique combination of maximum toughness and impact resistance with excellent high flow processability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPa50mm/min; ISO 527
Elongation at Break 45 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 5.0 %50mm/min; ISO 527
Tensile Modulus 1900 MPa1mm/min; ISO 527
Flexural Modulus 1800 MPaISO Data
Izod Impact, Notched (ISO) 80.0 kJ/m²ISO Test
 23.0 kJ/m²
@Temperature -40.0 °C
ISO Test
Charpy Impact Unnotched NBISO 179
 NB
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 9.00 J/cm²ISO 179
 2.80 J/cm²
@Temperature -30.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °C10 K/min
Deflection Temperature at 0.46 MPa (66 psi) 170 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °CISO 75
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedYes
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3Z HP BK20465 PA66 (Dry)
BASF Ultramid® A3Z HP UV PA66 (Dry)
BASF Ultramid® A3Z HP UV BK23220 PA66 (Dry)
BASF Ultramid® B3Z BK 30464 PA6 (Dry)
BASF Ultramid® A3L HP UV BK 23220 PA66 (Dry)

PBASF9275 / 85039

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.