MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NuSil Lightspan™ LS-8941 Silicone, Optical Adhesive Elastomer
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: General Purpose: Optical Adhesives and Elastomer

Comments: High Durometer to reduce tackiness, non-phenyl containing

Applications: Lenses made by Injecting or Compression Molding

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity >= 25000 cPB
 >= 27500 cPA
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength at Break 8.60 MPa
Elongation at Break 65 %
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.41
@Wavelength 589 nm
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 150 °C
Working Life >= 24.0 hour
 
Descriptive Properties
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil Lightspan™ LS-6140 Silicone, Optical Adhesive Elastomer
DuPont MOLYKOTE® 33 EXTREME LOW TEMPERATURE BEARING GREASE, LIGHT
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs
CHT Group QM 230 QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material

PNUSIL237 / 141961

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.