MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kao-Tab 95 Gun High Alumina Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Kao-Tab 95 Gun is a 95%-alumina castable designed for gunning. It maintains high strength throughout the temperature range of 3400°F (1871°C). Key features are high strength, high-use limit, good slag resistance, and high purity.

Features:

  • Designed for supercritical applications
  • Specially enhanced high alumina chemistries that allow Kao-Tab to outperform conventional castables
  • Applications:

  • Cat cracker transfer lines where more abrasion resistance is needed
  • Secondary ammonia reformer linings where low silica is desired
  • Recovery boiler
  • Upper furnace walls
  • Recovery/cyclone boilers
  • Lower furnace walls and floor
  • Cyclone boilers
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 2.628 - 2.804 g/cc0.09494 - 0.1013 lb/in³Fired
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.00965 - 0.0131 GPa1.40 - 1.90 ksiDried 18-24 hours at 220°F; ASTM C133
     0.00758 - 0.0124 GPa
    @Treatment Temp. 816 °C,
    Time 18000 sec
    1.10 - 1.80 ksi
    @Treatment Temp. 1500 °F,
    Time 5.00 hour
    ASTM C133
     0.00965 - 0.0138 GPa
    @Treatment Temp. 1870 °C,
    Time 18000 sec
    1.40 - 2.00 ksi
    @Treatment Temp. 3400 °F,
    Time 5.00 hour
    ASTM C133
    Compressive Strength 34.0 - 52.0 MPa4930 - 7540 psiDried for 18-24 hours at 220°F
     34.0 - 62.0 MPa4930 - 8990 psiFired 5 hours at 1500°F; ASTM C133
     41.0 - 62.0 MPa5950 - 8990 psiFired 5 hours at 3400°F
    Abrasion 13 - 2013 - 20loss, cc`s; Fired 5 hours at 1500°F; ASTM C704
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  1.61 W/m-K
    @Temperature 1370 °C
    11.2 BTU-in/hr-ft²-°F
    @Temperature 2500 °F
    ASTM C417
     1.74 W/m-K
    @Temperature 1090 °C
    12.1 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    ASTM C417
     1.92 W/m-K
    @Temperature 816 °C
    13.3 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    ASTM C417
     2.20 W/m-K
    @Temperature 538 °C
    15.3 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    ASTM C417
     2.61 W/m-K
    @Temperature 260 °C
    18.1 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    ASTM C417
    Maximum Service Temperature, Air 1870 °C3400 °F
    Shrinkage  0.10 - 0.30 %
    @Temperature 816 °C,
    Time 18000 sec
    0.10 - 0.30 %
    @Temperature 1500 °F,
    Time 5.00 hour
    ASTM C113
     0.00 - 1.5 %
    @Temperature 1870 °C,
    Time 18000 sec
    0.00 - 1.5 %
    @Temperature 3400 °F,
    Time 5.00 hour
    ASTM C113
     0.00 - 0.20 %
    @Treatment Temp. 104 °C
    0.00 - 0.20 %
    @Treatment Temp. 220 °F
    Dried 18-24 hours; ASTM C113
     
    Processing PropertiesMetricEnglishComments
    Shelf Life 12.0 Month12.0 Month
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 95 %95 %
    Alkalis 0.10 %0.10 %
    CaO 4.2 %4.2 %
    Fe2O3 0.20 %0.20 %
    SiO2 0.20 %0.20 %
     
    Descriptive Properties
    MgO Contenttraces
    TiO2 contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Chosun Refractories SAL85BR Special High Alumina brick
    Chosun Refractories H-4S High Alumina brick
    Chosun Refractories H-4 High Alumina brick
    Chosun Refractories H-3S High Alumina brick
    Chosun Refractories H-2 High Alumina brick

    CTHERM069 / 2389

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.