MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

KLJ Group KLJ XL 01 FC XLPE Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: The base material KLJ XL 01 FC is based on poly-ethylene and chemically grafted with Silane. KLJ XL MB 02 FC contains the catalyst additive, when mixed graft materials, it accelerates the cross-linking reaction in open atmosphere at normal temperature and humidity condition. This material is suitable to be used for cable up to 6KV (Ambient curing)

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 21.0 MPa>= 3050 psi
 >= 22.26 MPa>= 3229 psi
Elongation at Break >= 600 %>= 600 %IS 10810 Part-7
 >= 300 %
@Treatment Temp. -30.0 °C
>= 300 %
@Treatment Temp. -22.0 °F
Cold Elongation; % IS 10810 Part-11
 >= 570 %
@Treatment Temp. 132 - 138 °C,
Time 605000 sec
>= 570 %
@Treatment Temp. 270 - 280 °F,
Time 168 hour
% IS 10810 Part-11
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 3.00e+15 ohm-cm
@Temperature 27.0 °C
>= 3.00e+15 ohm-cm
@Temperature 80.6 °F
IS 3396
Dielectric Constant <= 1.7<= 1.7IEC 60250
Dielectric Strength >= 30.0 kV/mm>= 762 kV/inIEC 60243
Dissipation Factor <= 0.00020<= 0.00020IEC 60250
 
Thermal PropertiesMetricEnglishComments
Shrinkage <= 1.3 %
@Temperature 127 - 133 °C,
Time 3600 sec
<= 1.3 %
@Temperature 261 - 271 °F,
Time 1.00 hour
IS 7098
 
Processing PropertiesMetricEnglishComments
Zone 1 115 - 145 °C239 - 293 °F
Zone 2 135 - 165 °C275 - 329 °F
Zone 3 155 - 185 °C311 - 365 °F
Zone 4 175 - 205 °C347 - 401 °F
Zone 5 185 - 215 °C365 - 419 °F
Die Temperature 190 - 220 °C374 - 428 °F
Head Temperature 190 - 220 °C374 - 428 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Content600 ppmASTM D1045
Hot Set<100%200°C/15 minute 20N/cm2, (Thickness 1.0 mm/24Hrs), IS 18010 Part-30
Permanent Set after cooling<2.5%IS 18010 Part-30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKLJ338 / 284359

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.