MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay MIRACARE® BC-34 Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: Ultra mild, economy concentrate for use in the preparation of tear-free cleansing products

Chemical Name: PERFORMANCE CONCENTRATE BLEND

CAS: 70851-07-9, 25446-78-0, 56-81-5

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRACARE© BC-34 is a formulated surfactant concentrate specially developed to yield ultra mild, tear free personal care products. An optimized blend of high foaming surfactants and proven anti-irritation agents, MIRACARE© BC-34 readily forms clear, non irritating systems with simple water dilution. MIRACARE© BC-34 is ideally suited for use in the preparation of tear free baby shampoos, children’s bath and toiletries, facial cleansers, and related cleansing products where mildness is required.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 41 - 44 %
@Temperature 105 °C,
Time 7200 sec
41 - 44 %
@Temperature 221 °F,
Time 2.00 hour
Oven, Sand; RP-0544
pH 5.5 - 7.05.5 - 7.0RP-0420
Viscosity <= 5000 cP<= 5000 cP#3 SP @ 20 rpm; RP-0596
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 4.0<= 4.0RP-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceClear to Slightly Hazy LiquidRP-0064

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD237 / 137468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.