MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Exceed™ 1018 MF Film Grade Hexene LLDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Exceed™ performance PE polymers Used to formulate a wide range of film structures offering superior mechanical performance for highly demanding end-use applications.  Exceed 1018 is an ethylene 1-hexene copolymer resin.  Films made from these resins have outstanding tensile, impact strength, impact strength, and puncture.  These superior strength properties, along with excellent drawability, allow down gauging in bag applications.   TnPP is not intentionally added to Exceed 1018. 

Availability: North America. 

Additive:   antiblock: 4500 ppm; slip: 450 ppm; processing aide: yes; thermal stabilizer: yes. 

Applications:  agricultural film, freezer film, packaging films, bag in box, general packaging, premium trash bags, barrier food packaging, heavy duty bags, stand up pouches, blown film, industrial packaging, trash bags, bread bags, lamination film, trash can liners; food packaging, multilayer packaging film, form fill and seal packaging, overwrap film.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.65 MPa1400 psiASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa1400 psiASTM D882
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 600 %600 %ASTM D882
Puncture Energy 1.81 J1.33 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 250 g250 gASTM D1922
Elmendorf Tear Strength TD 470 g470 gASTM D1922
Dart Drop Test 460 g1.01 lbASTM D1709A
Film Tensile Strength at Break, MD 54.5 MPa7900 psiASTM D882
Film Tensile Strength at Break, TD 42.7 MPa6200 psiASTM D882
1% Secant Modulus, MD 186 MPa27000 psiASTM D882
1% Secant Modulus, TD 193 MPa28000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 119 °C247 °FPeak; ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 18 %18 %ASTM D1003
Gloss 29 %29 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade
ExxonMobil Exceed™ 1018 MJ Film Grade Hexene LLDPE
ExxonMobil Exceed™ 1015MA Film Grade Hexene LLDPE

PEX98850 / 238232

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.