MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haynes Hastelloy® W alloy as a weld filler, base metal Multimet alloy 12.7 mm plate weldment
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemical process industries.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: AWS A5.14, ASME SFA 5.11, ASME SFA 5.14, AMS 5755, AMS 5786, AMS 5787, AWS A5.11
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 9.00 g/ccat RT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 800 MPa
 290 MPa
@Temperature 870 °C
Tensile Strength, Yield 425 MPa
 215 MPa
@Temperature 870 °C
Elongation at Break 49 %Failures in base metal.
 28 %
@Temperature 870 °C
Failures in base metal.
Reduction of Area 65 %Failures in base metal.
 42 %
@Temperature 870 °C
Failures in base metal.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.2 µm/m-°C
@Temperature 20.0 - 600 °C
 13.2 µm/m-°C
@Temperature 20.0 - 500 °C
 13.5 µm/m-°C
@Temperature 20.0 - 700 °C
 14.2 µm/m-°C
@Temperature 20.0 - 800 °C
 14.8 µm/m-°C
@Temperature 20.0 - 900 °C
 15.3 µm/m-°C
@Temperature 20.0 - 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.12 %
Chromium, Cr 5.0 %
Cobalt, Co 2.5 %
Iron, Fe 6.0 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo 24 %
Nickel, Ni 63 %
Silicon, Si <= 1.0 %
Vanadium, V <= 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek MTEK CW-12MW Cast UNS N30002 Severe Corrosion and Heat Resistant Alloy
MetalTek MTEK CW-2M Cast UNS N26455 Severe Corrosion and Heat Resistant Alloy
MetalTek MTEK CX-2MW Cast UNS N26022 Severe Corrosion and Heat Resistant Alloy
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
Haynes Hastelloy® B-3® alloy, after elevated temperature exposure

NHAWAQ / 17010

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.