Acrylic copolymer adhesive with silicone treated release paper liner. Features: - Excellent adhesion to low surface energy substrates
- Compatible with most printing inks
Applications: Mounting a wide variety of substrates where quick adhesion is critical including coarse, uneven materials, low surface energy films and reverse printed materials. Information provided by Dielectric Polymers. |