MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cray Valley Ricobond® 1756 Polybutadiene Adducted with Maleic Anhydride
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Ricobond® 1756 is a low molecular weight, high vinyl butadiene functionalized with maleic anhydride, allowing enhanced adhesion of rubber compounds to metal and textiles. The anhydride functionality can react with epoxy, amine, and hydroxyl groups, while the vinyl functionality is peroxide curable, enabling the creation of unique adhesives, sealants, encapsulants, and coatings.

Product Highlights / Performance Properties:

  • Excellent reactivity
  • Adhesion promoter
  • Compatibility with polar and non-polar materials
  • Moisture resistance
  • Low temperature tackifier
  • Reactive toughener for epoxies
  • Reactive compatibilizer for thermoplastics
Suggested Applications:
  • Elastomers
  • Coatings
  • Electronics
  • Encapsulants
  • Sealants
  • Adhesives
  • Compatibilizers

Information provided by Cray Valley

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/ccQCS-649
Viscosity 140000 cP140000 cPQCS-630
Molecular Weight 2500 g/mol2500 g/molQCS-651
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -18.0 °C-0.400 °FQCS-681
 
Descriptive Properties
1,2 Vinyl0.7QCS-642
Groups/Chain3MA, QCS-660

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCRAYV020 / 316173

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.