MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Tritan™ Renew EX401-50 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Tritan™ Renew copolyester EX401-50, specifically developed for the Infant Care market, is an amorphous copolyester with excellent appearance and clarity. Tritan Renew EX401-50 contains a mold release derived from vegetable based sources. Its most outstanding features are clarity, excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan Renew EX401-50 meets infant care sterilization requirements via boiling water or microwave steam sterilization. This new-generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity, and aggressive cleaning agents. Tritan Renew EX401-50 can be converted into parts using injection molding, injection stretch blow molding (ISBM), and extrusion blow molding techniques. Tritan Renew EX401-50 may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Contact Eastman representative for details on global food contact regulatory clearances. Tritan Renew EX401-50 is included in Eastman Chemical Company’s Customer Notification Procedure which details our policy for customer notification when significant changes are made in Tritan Renew EX401-50 sold into the infant care market. This procedure provides the infant care industry an added layer of confidence in the consistent quality and performance of Tritan™ Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Baby bottles/sippy cups
  • Childcare items
  • Infant/toddler
Key Attributes
  • Chemical resistance
  • Clarity
  • Global food contact regulatory clearances
  • Heat resistance
  • Hydrolytic stability
  • Impact resistance
  • Processing ease
  • Sterilization capable via steaming or boiling water

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Linear Mold Shrinkage 0.00500 - 0.00700 in/inInjection; ASTM D955
 0.0120 - 0.0160 in/inBlow Mold Shrinkage
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ASTM D785
Tensile Strength at Break 49.0 MPaISO 527
 53.0 MPaASTM D638
Tensile Strength, Yield 44.0 MPaASTM D638
 44.0 MPaAfter 8 hr boiling
 45.0 MPaISO 527
 45.0 MPaAfter re-equilibration
Elongation at Break 130 %ISO 527
 140 %ASTM D638
Elongation at Yield 6.50 %After re-equilibration
 7.00 %ISO 527
 7.00 %ASTM D638
 7.00 %After 8 hr boiling
Tensile Modulus 1585 MPaASTM D638
 1624 MPaISO 527
Flexural Yield Strength 66.0 MPaASTM D790
Flexural Modulus 1531 MPaISO 178
 1585 MPaASTM D790
Izod Impact, Notched 643 J/mAfter re-equilibration
 650 J/mAfter 8 hr boiling
 126 J/m
@Temperature -40.0 °C
ASTM D256
 650 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Puncture Energy 59.0 J
@Temperature 23.0 °C
ASTM D3763
 63.0 J
@Temperature -40.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 109 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze <= 1.00 %ASTM D1003
 <= 1.00 %After 8 hr boiling
Transmission, Visible 92.0 %Total; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 90.0 °CBlow Mold Temperature
 185 - 195 °CPreform Temperature at Blow
Melt Temperature 240 - 250 °CExtrusion Blow Molding
 260 - 282 °CInjection Molding
 270 - 285 °CInjection Stretch Blow Molding
Mold Temperature 25.0 - 45.0 °CExtrusion Blow Molding
 38.0 - 66.0 °CInjection Molding
 60.0 - 70.0 °CInjection Stretch Blow Molding
Drying Temperature 88.0 °CTypical
Dry Time 4.00 - 6.00 hourTypical
Dew Point <= -35.0 °CTypical
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details
 
Descriptive Properties
Blow Pressure0.03-0.08 MPaPrimary
 0.2-0.3 MPaSecondary

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4203 / 323826

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.