MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Dowlex™ 2645.11S PE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Dowlex™ 2645.11S Polyethylene Resin is designed for the production of a wide variety of film applications. Films made from this resin exhibit a combination of good toughness and tear resistance.
Complies with: FDA FCN 741; EU. No 10/2011.
Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: 3000 ppm; Processing Aid: No; Slip: 1200 ppm

Agency Ratings: FDA FCN 741; EU No 10/2011

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D792
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 3000 ppm
Slip Level 1200 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 2060 psi
@Thickness 0.0508 mm
ASTM D882
Film Tensile Strength at Yield, TD 2120 psi
@Thickness 0.0508 mm
ASTM D882
Film Elongation at Break, MD 660 %
@Thickness 0.0508 mm
ASTM D882
Film Elongation at Break, TD 740 %
@Thickness 0.0508 mm
ASTM D882
2% Secant Modulus 24400 psi
@Thickness 0.0508 mm
MD; ASTM D882
 34500 psi
@Thickness 0.0508 mm
TD; ASTM D882
Elmendorf Tear Strength MD 720 g
@Thickness 0.0508 mm
ASTM D1922
Elmendorf Tear Strength TD 1000 g
@Thickness 0.0508 mm
ASTM D1922
Dart Drop Test 300 gASTM D1709A
Film Tensile Strength at Break, MD 7080 psi
@Thickness 0.0508 mm
ASTM D882
Film Tensile Strength at Break, TD 5680 psi
@Thickness 0.0508 mm
ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 248 °F
Vicat Softening Point 225 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 14 %
@Thickness 0.0508 mm
ASTM D1003
Gloss 56 %
@Thickness 0.0508 mm
45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
Film Puncture Resistance80 ft-lb/in32.0 mil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF418 / 311111

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.