MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chevron Phillips MC3100 High Heat Crystal Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Description

Chevron MC3100 is a high heat polystyrene designed to offer a good balance of moldability, exceptional easy release from the mold, and physical properties for applications requiring clarity and high heat distortion temperature. Chevron MC3100 natural complies with Food Additive Regulation 21CFR177.1640 for polystyrene and rubber modified polystyrene, which states that such materials may be safely used in contact with foods.

Applications

Chevron MC3100 is one of the clearest polystyrene resins available in the industry. Typical applications include vials, jars and bottles.Information provided by Chevron Phillips Chemical Company.

The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Melt Flow 3.0 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7800 psiat 2.0 in/min; ASTM D638
Tensile Strength, Yield 7800 psiat 2.0 in/min; ASTM D638
Elongation at Break 4.5 %ASTM D638
Tensile Modulus 460000 psiASTM D638
Flexural Strength 12000 psiASTM D790B
Flexural Modulus 450000 psiASTM D790B
Izod Impact, Notched 0.250 ft-lb/in1/4 in.; ASTM D256
 0.350 ft-lb/in1/8 in.; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 196 °FASTM D648
Vicat Softening Point 226 °FASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Americas Styrenics STYRON® 685D High Heat Crystal Polystyrene
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe)
Ineos Nova 1210 High Heat Crystal Polystyrene
Ineos Nova 1504 High Heat Crystal Polystyrene

PPSRA19 / 58249

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.