MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Surlyn® SG201U NC010 Supergloss Molding Alloy
Categories: Polymer; Thermoplastic

Material Notes: Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, and provides improved scratch and abrasion resistance. Surlyn® SG201U is an excellent, lower cost, more environmentally friendly alternative to painting.

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.043 g/ccASTM D792
Linear Mold Shrinkage 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 44.8 MPaASTM D638
Elongation at Break >= 200 %ASTM D638
Flexural Modulus 1.139 GPaASTM D790
Izod Impact, Notched 5.00 ft-lb/in
@Temperature -30.0 °C
ASTM D256
 12.0 ft-lb/in
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 190 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 235 - 250 °C
Mold Temperature 105 - 175 °F
Drying Temperature <= 175 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® 1650SB
Dow Surlyn® 8945 Thermoplastic Ionomer Resin
Dow Surlyn® 9945 Thermoplastic Ionomer Resin
Dow Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating

PDUPM103 / 33770

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.