MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta NP193PM Phenolic Laminate Sheet
Categories: Polymer; Thermoset; Phenolic

Material Notes: NP193PM is composed of a 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temperature phenolic resin matrix which includes a non-conducting solid lubricant. This composite has excellent mechanical strength at elevated temperatures and adverse environments. Applications include wear plates for conveyor systems, valve plates, and compressor and pump vanes.

Information provided by Norplex-Micarta

Key Words: Aramid, Phenolic, Micarta, Molybdenum Disulfide Lubricant
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.54 g/cc
@Thickness 12.7 mm
1.54 g/cc
@Thickness 0.500 in
ASTM D792
Moisture Absorption 1.94 %
@Thickness 1.57 mm
1.94 %
@Thickness 0.0620 in
ASTM D570 Condition A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 95
@Thickness 6.35 mm
95
@Thickness 0.250 in
ASTM D785
Tensile Strength  66.9 MPa
@Thickness 3.17 mm
9700 psi
@Thickness 0.125 in
CrossWise; ASTM D638 Condition A
 177 MPa
@Thickness 3.17 mm
25600 psi
@Thickness 0.125 in
LengthWise; ASTM D638 Condition A
Flexural Strength  121 MPa
@Thickness 1.57 mm
17500 psi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 253 MPa
@Thickness 1.57 mm
36700 psi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Compressive Strength 281 MPa
@Thickness 12.7 mm
40700 psi
@Thickness 0.500 in
Flatwise; ASTM D695 Condition A
Izod Impact, Unnotched  3.90 J/cm
@Thickness 12.7 mm
7.30 ft-lb/in
@Thickness 0.500 in
CrossWise; ASTM D256 Condition E-48/50
 12.2 J/cm
@Thickness 12.7 mm
22.9 ft-lb/in
@Thickness 0.500 in
LengthWise; ASTM D256 Condition E-48/50
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
@Thickness 3.17 mm
15.0 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 39.8 µm/m-°C
@Thickness 3.17 mm
22.1 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
UL RTI, Mechanical with Impact 165 °C329 °FUL Bulletin 746b
 
Descriptive Properties
Bonding Strength2400[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Zelux® GS Polycarbonate - Gamma Stabilized For Medical Applications
LE Phenolic Laminate
Norplex-Micarta NP101 Phenolic Nylon Laminate Sheet
Ensinger Hydex™ 301 Rigid Polyurethane (PU)
G-3 Fiberglass Phenolic Laminate Sheet

PNORPM071 / 192828

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.