MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond Supreme 70CN Two component, toughened epoxy system for bonding, sealing, coating and potting derived from natural substances
Categories: Polymer; Thermoset; Epoxy

Material Notes: Master Bond Supreme 70CN is a moderate viscosity, toughened epoxy for high performance bonding, sealing, coating and potting. The mix ratio is a forgiving 100 to 30 by weight with a user friendly working time of 60-90 minutes. It cures readily at ambient temperatures and more rapidly at elevated temperatures. An optimum curing schedule is overnight at room temperature followed by 4-5 hours at 140-170°F. Supreme 70CN does not contain any solvents or diluents and has low shrinkage upon curing. It should be noted that this epoxy has exceptional wetting properties. Supreme 70CN is an excellent adhesive and bonds well to a wide variety of substrates including metals, ceramics and many rubbers, plastic materials, and especially composites. An important feature is its toughness, which allows it to be used for bonding dissimilar substrates and to withstand thermal cycling. Other favorable attributes include good physical strength and excellent chemical resistance. It is a reliable electrical insulator, which combined with its lower exotherm, enables it to be utilized in a wide array of potting applications. The service temperature range is -100°F to +400°F. The color of Part A is black and Part B is light orange. This multi-faceted system can be considered for applications in aerospace, electronic, opto-electronic and specialty type OEM, particularly those involving composites and fibers.

Product Advantages:

  • Moderate viscosity and longer open time
  • Fine physical strength properties
  • Toughened system; resists thermal cycling
  • Outstanding chemical resistance
  • NASA low outgassing
Key Features:
  • Moderate viscosity
  • Superior chemical resistance
  • Black colored, optically opaque
  • NASA low outgassing

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 1000 - 3000 cP1000 - 3000 cPPart B
 8000 - 12000 cP8000 - 12000 cPMixed viscosity
 70000 - 120000 cP70000 - 120000 cPPart A
Linear Mold Shrinkage <= 0.00010 cm/cm<= 0.00010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8575 - 85
Tensile Strength 68.9 - 75.8 MPa10000 - 11000 psi
Tensile Modulus 2.07 - 2.41 GPa300 - 350 ksi
Adhesive Bond Strength 6.89 - 8.27 MPa1000 - 1200 psiTensile lap shear, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.5
@Frequency 60 Hz
4.5
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 - 40.0 µm/m-°C19.4 - 22.2 µin/in-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -73.0 °C-99.4 °F
Glass Transition Temp, Tg 125 - 130 °C257 - 266 °Fwith post cure
 
Processing PropertiesMetricEnglishComments
Cure Time  180 - 240 min
@Temperature 71.1 - 93.3 °C
3.00 - 4.00 hour
@Temperature 160 - 200 °F
Option 2
 240 - 300 min
@Temperature 60.0 - 76.7 °C
4.00 - 5.00 hour
@Temperature 140 - 170 °F
Optimal: overnight at 75°F plus 4-5 hours at 140-170°F
 5760 - 7200 min
@Temperature 23.9 °C
96.0 - 120 hour
@Temperature 75.0 °F
Option 1
Working Life 60.0 - 90.0 min60.0 - 90.0 min
Shelf Life 1.00 Month1.00 Monthin cans
 6.00 Month6.00 Monthin syringes
 
Descriptive Properties
Mixing ratio100:30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM644 / 268832

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.