MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Unitika RUN35-C25 PA6, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: High modulus and low warpage nylon

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.66 g/cc0.0600 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.0 %1.0 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
@Thickness 3.20 mm
0.0010 in/in
@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 3.20 mm
0.0050 in/in
@Thickness 0.126 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 164 MPa23800 psiISO 527-1/-2
Elongation at Break 1.3 %1.3 %ISO 527-1/-2
Tensile Modulus 17.5 GPa2540 ksiISO 527-1/-2
Flexural Strength 240 MPa34800 psiISO 178
Flexural Modulus 15.0 GPa2180 ksiISO 178
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²ISO 179-1
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 µm/m-°C8.33 µin/in-°FISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 194 °C381 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 191 °C376 °FISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SGL Carbon Group SIGRAFIL C® C25 S003 PUT Staple Carbon Fiber, Polyurethane Sizing
SGL Carbon Group EK 24 Carbon Graphite
Celanese Zenite® 6330 BK010 LCP (Extended Tabular Temperature Data)
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
303 Stainless Steel, annealed

PUNITIK823 / 177845

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.