MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Hostacom TRC 787N C1 C15102 Thermoplastic Olefinic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hostacom TRC787N C1 C15102 is high melt flow, mineral-filler filled thermoplastic elastomeric olefin(TEO) resin, has an excellent balance of processability, rigidity, and impact and scratch and mar resistance. It can be used for automotive interior applications, such as instrument panel, console, glove box. This grade is available for color-matched, pellet form. Applications: Instrument Panels, Interior Trims

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Melt Flow 21 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 17.5 MPaISO 527-1,-2
Flexural Modulus 1800 MPaTech.A; ISO 178/A1
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 48.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
LyondellBasell Hostacom TRC787N 600R JET BLK Thermoplastic Olefinic Elastomer
DuPont Mobility and Materials Zytel® ST801 BK010A PA66-HI
Trinseo MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
LyondellBasell Hostacom TRC 787N E1 D71499 Polypropylene with 20% Talc Filler

PEQT8323 / 219958

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.