MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BEC Materials SEBS 501T
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Thermoplastic elastomer SEBS polymer YH-501T is a low-molecular weight, liner Styrene Ethylene Butylene Styrene Block Copolymer . It can be applied to hot melt adhesive (pressure-sensitive adhesive), plastic modification and so on due to its good fluidity and low melt viscosity.

Application: Adhesives/Coating/Plastic modification

Formula: Sealant (Parts by mass)
SEBS polymer (YH-501T): 100
C5 Resin: 100-180
Maleic Anhydride Modified Poly Butylene: 50-100
Naphthenic Oil: 100-300
Toluene:Ethyl Acetate(1:1): 60-150

Information provided by BEC Materials, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %
Viscosity 400 - 800 cP400 - 800 cPSolution, 20%
 
Chemical PropertiesMetricEnglishComments
Styrene Content 30 %30 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 68>= 68
Tensile Strength >= 16.0 MPa>= 2320 psi
Elongation at Break >= 450 %>= 450 %
300% Modulus >= 3.00 MPa>= 435 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBECM071 / 307024

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.