MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Braskem UTEC6541 Ultra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: UTEC6541 is an Ultra High Molecular Weight Polyethylene with a molecular weight greater than 10 times higher than HDPE resins. This extremely high molecular weight yields several unique properties to this polymer such as high abrasion resistance, impact strength, and because it is a self-lubricating material, a low coefficient of friction.
Applications: Applications which require highest wear resistance and the use of pigments and/or additives, Technical parts RAM extruded and compression molded sheets, rods and profiles.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.450 g/cc0.0163 lb/in³ASTM D1895
Density 0.925 g/cc0.0334 lb/in³ASTM D792
Particle Size 160 µm160 µmAverage. Dp50; Laser Light Scattering
Viscosity Test 2800 cm³/g28 dl/gIntrinsic; ASTM D4020
Molecular Weight 8.00e+6 g/mol8.00e+6 g/molaverage; Braskem Test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 58
@Time 15.0 sec
>= 58
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break >= 30.0 MPa>= 4350 psiASTM D638
Tensile Strength, Yield >= 17.0 MPa>= 2470 psiASTM D638
Elongation, Ultimate >= 350 %>= 350 %ASTM D638
Charpy Impact, Notched >= 10.0 J/cm²>= 47.6 ft-lb/in²Double-notched specimens (14º v-notch on both sides); ISO 11542-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D257
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °FASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS663 / 314056

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.