MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior Durethan® DP BKV 35 XF 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: 35% glass fiber, extreme flow

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.358 g/cc0.04906 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0016 cm/cm0.0016 in/in150x105x3; ISO 2577
 0.0022 cm/cm0.0022 in/in60x60x2; ISO 2577
Linear Mold Shrinkage, Transverse 0.0058 cm/cm0.0058 in/in60x60x2; ISO 2577
 0.0087 cm/cm0.0087 in/in150x105x3; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa23900 psi5 mm/min; ISO 527-1,-2
Elongation at Break 2.9 %2.9 %5 mm/min; ISO 527-1,-2
Tensile Modulus 9.50 GPa1380 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 250 MPa36300 psi2 mm/min; ISO 178-A
Flexural Yield Strength 250 MPa
@Strain 3.5 %
36300 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 8.70 GPa1260 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 3.7 %3.7 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 14.0 kJ/m²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) 75.0 kJ/m²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 220 °C428 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 209 °C408 °FISO 75-1,-2
Shrinkage, MD  0.030 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.030 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction 150x105x3; ISO 2577
 0.050 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.050 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction; 60x60x2; ISO 2577
Shrinkage, TD  0.020 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.020 %
@Treatment Temp. 248 °F,
Time 4.00 hour
150x105x3; ISO 2577
 0.14 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.14 %
@Treatment Temp. 248 °F,
Time 4.00 hour
60x60x2; ISO 2577
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °F
Mold Temperature 80.0 °C176 °F
Back Pressure 60.0 MPa8700 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANW9532 / 208358

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.