MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled

Material Notes: Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensional stability even under severe environmental conditions. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS)

Processing: Compression, Injection and transfer molding

Applications: Pin and socket connectors, Spools, Potentiometers, Switches

Information provided by Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.90 - 2.10 g/ccISO 1183
Apparent Bulk Density 0.750 - 0.900 g/ccISO 60
Water Absorption <= 0.20 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cmInjection; ISO 2577
 0.0050 - 0.0060 cm/cmCompression; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 35.0 - 60.0 MPaCompression; ISO 527
 40.0 - 70.0 MPaInjection; ISO 527
Modulus of Elasticity 6.00 - 9.00 GPaCompression; ISO 527
 9.00 - 11.0 GPaInjection; ISO 527
Flexural Strength 80.0 - 100 MPaCompression; ISO 178
 100 - 140 MPaInjection; ISO 178
Flexural Modulus 8.00 - 12.0 GPaCompression; ISO 178
 13.0 - 16.0 GPaInjection; ISO 178
Compressive Strength 150 - 200 MPaISO 604
Charpy Impact Unnotched 5.00 - 10.0 kJ/m²Compression; ISO 179/1eU
 8.00 - 11.0 kJ/m²Injection; ISO 179/1eU
Charpy Impact, Notched 2.50 - 3.50 kJ/m²Compression; ISO 179/1eA
 3.50 - 5.00 kJ/m²Injection; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 - 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 - 1.00e+15 ohmIEC 60093
Dielectric Constant 4.0 - 4.5
@Frequency 1e+6 Hz
IEC 60250
 4.5 - 5.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 - 40.0 kV/mmIEC 60243-1
Dissipation Factor 0.010 - 0.030
@Frequency 100 Hz
IEC 60250
 0.010 - 0.030
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 180 - 240 secASTM D495
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 5.00 - 10.0 µm/m-°C
@Temperature 50.0 - 100 °C
ISO 11359-2
Thermal Conductivity 0.900 - 1.10 W/m-KASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75-A
Deflection Temperature at 8.0 MPa >= 180 °CISO 75-C
Flammability, UL94 V-0
@Thickness 0.800 mm
Shrinkage <= 0.050 %
@Temperature 110 °C,
Time 605000 sec
Post shrinkage; ISO 2577
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 15.0 - 25.0 °C
 
Descriptive Properties
Glow wire flammability test960/1IEC 60695 2-12
Glow wire ignitability test930/1IEC 60695 2-13
Water Absorption<15 mg24 hr, 23°C; ISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
Overview of materials for Nylon 66, Impact Grade
Overview of materials for Nylon 612, Glass Fiber Filler
Overview of materials for Nylon 46, Glass Fiber Reinforced

PRASCI28 / 179165

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.