MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Belsil® ADM 1650 Amodimethicone
Categories: Fluid; Polymer

Material Notes: BELSIL® ADM 1650 is a non-reactive aminofunctional polydimethylsiloxane with an average viscosity of 1000 mm2/s. When used in acidic shampoos, hair rinses and hair formulations, its amine group is protonated and a cationic polymer is obtained. This polymer readily coats the negatively charged surface of the hair, providing excellent conditioning properties.

Application: The major field of application for BELSIL® ADM 1650 is hair care. The non-reactive amino-functional silicone fluid forms a protective sheath around the hair fiber that lasts through several shampooing cycles. BELSIL® ADM 1650 Amodimethicone is used mainly in shampoos and hair conditioners. The conditioning properties are highly effective in these applications, resulting in improved wet and dry compatibility and a pleasant, soft feel.

INCI name: Amodimethicone

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1000 cPdynamic
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Available in multiple densities
 
Descriptive Properties
Amine number0.6 mmol/g
Appearanceclear, colorless
SolubilityBELSIL® DM 1 Plus>10%
 BELSIL® DM 10>10%
 BELSIL® DM 125001-10%
 BELSIL® DM 350>10%
 BELSIL® DM 5>10%
 BELSIL® DM 600001-10%
 BELSIL® PDM 1000insoluble
 BELSIL® PDM 20>10%
 BELSIL® PDM 350 VP1-10%
 C12-15 alkyl benzoatesinsoluble
 C9-13 isoparaffins1-10%
 Castor oilinsoluble
 Cyclopentasiloxane>10%
 Decyl oleateinsoluble
 Ethanolinsoluble
 Ethyl acetate>10%
 Glycerininsoluble
 Isopropanol>10%
 Isopropyl myristate>10%
 Lanolin oilinsoluble
 Mineral oil (high-viscosity)insoluble
 Mineral oil (low-viscosity)insoluble
 Octyldodecanolinsoluble
 Oleyl alcoholinsoluble
 Oleyl oleateinsoluble
 Olive oilinsoluble
 Propylene glycolinsoluble
 Waterinsoluble
 Wheat germ oilinsoluble
Structurelinear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Belsil® ADM 9000 E Amino-Functional Silicone
Wacker Belsil® ADM 1370 Amino-Functional Silicone
Wacker Wacker® Finish CT 34 E Silicone Softener Emulsion
Wacker Belsil® ADM 8301 E Amino-Functional Silicone
Wacker Belsil® ADM 6300 E Amino-Functional Silicone

PWACK9002 / 204531

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.