MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Project 00NK02738) for UL Standard 94. EP1295 Black qualifies for a vertical burn rating of V-0 at 6.1 mm thickness. It also gives very good resistance to water, salt spray, inorganic acids and bases and most organic solvents. It cures quickly at room temperature to a tough, semi-rigid polymer. It has good wetting and adhesion to most surfaces and is free flowing to penetrate voids and give good air release. EP1295 Black was formulated to a 1/1 volume mix ratio for ease of use in automatic mixing equipment with static mixers. It contains soft, low-abrasion fillers which can separate over time, although they have good resistance to hard settling. If used in side-by-side cartridge format, they should be stored at 5C, rotating stock on a FIFO basis. EP1295 Black will generally reach handle cure at room temperature within 16 to 24 hours depending upon mass and ambient temperature. Full cure usually achieved within 48 – 72 hours. Cure time can be accelerated by the application of heat after product has gelled. Times and temperatures from 2 hours at 60°C to 30 minutes at 100°C are typical for most castings (less than 100 grams).

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/ccPart B; TM R050-16
 1.39 g/ccMixed; TM R050-16
 1.46 g/ccPart A; TM R050-16
Water Absorption 0.56 %
@Time 86400 sec
TM R050-35
Viscosity 8500 cPPart A, RVT, #4, 10 rpm.; TM R050-12
 13500 cPPart B, RVT, #4, 10 rpm.; TM R050-12
 11000 cP
@Shear Rate 1.00 1/s
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55
Tensile Strength at Break 750 psiTM R050-36
Tensile Strength, Ultimate 750 psiTM R050-36
Tensile Strength, Yield 150 psiTM R050-36
Elongation at Break 18 - 22 %TM R050-36
Tensile Modulus 3.00 - 5.00 ksiTM R050-36
Compressive Yield Strength 450 psiTM R050-38
Compressive Strength 2000 psiBreak; TM R050-38
 5000 psiUltimate; TM R050-38
Compressive Modulus 8.00 - 10.0 ksiTM R050-38
Adhesive Bond Strength 850 psiLap Shear-Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.20e+12 ohm-cm
Dielectric Constant 4.8
@Frequency 100000 Hz
 6.6
@Frequency 100 Hz
Dielectric Strength 410 V/mil
Dissipation Factor 0.060
@Frequency 100000 Hz
 0.20
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature <=10.0 °C
Below Tg
 175 µm/m-°C
@Temperature >=10.0 °C
Above Tg
Thermal Conductivity 0.300 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 10.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 60.0 °C
 24.0 - 48.0 hour
@Temperature 25.0 °C
Pot Life 10.0 min
 
Descriptive Properties
Appearanceblack liquid
Mix Ratio1.08:1Weight
 1:1Volume
Side-By-Side Cartridges CapableYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP1200LV Casting Resin
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive
Resinlab® SEC1233 Silver Filled Epoxy Adhesive

PRESL129 / 101543

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.