MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Keltan® 4577 Ethylene-Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Crystalline ethylene-propylene rubber with medium ENB (ethylidene norbornene) content and a medium Mooney viscosity at 75 phr extender oil. The combination of very high molecular weight and high green strength results in a very high level of physical properties and contributes to an excellent collapse resistance in extruded profiles. Typical applications are in automotive profiles, TPV and (low hardness) molded goods.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/cc
Mooney Viscosity 46
@Temperature 125 °C
(1+4); ISO 289
 
Descriptive Properties
Content5.1 percentENB, ASTM D6047
 66 percentEthylene, ASTM D3900
 75 phrOil, ISO 1407

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess Keltan® 3050 Ethylene-Propylene Rubber
Lanxess Keltan® 2470L Ethylene-Propylene Rubber
Lanxess Keltan® 3973 Ethylene-Propylene Rubber
Lanxess Keltan® 5465Q Ethylene-Propylene Rubber
Lanxess Keltan® 2450S Ethylene-Propylene Rubber

PLANY8567 / 208960

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.