MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 188/ Multimet alloy 12.7 mm plate weldments
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemical process industries.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: AWS A5.14, ASME SFA 5.11, ASME SFA 5.14, AMS 5755, AMS 5786, AMS 5787, AWS A5.11
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.00 g/ccat RT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 805 MPa
 320 MPa
@Temperature 870 °C
Tensile Strength, Yield 455 MPa
 235 MPa
@Temperature 870 °C
Elongation at Break 35 %Failures in base metal.
 19 %
@Temperature 870 °C
Failures in base metal.
Reduction of Area 64 %Failures in base metal.
 19 %
@Temperature 870 °C
Failures in base metal.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.2 µm/m-°C
@Temperature 20.0 - 600 °C
 13.2 µm/m-°C
@Temperature 20.0 - 500 °C
 13.5 µm/m-°C
@Temperature 20.0 - 700 °C
 14.2 µm/m-°C
@Temperature 20.0 - 800 °C
 14.8 µm/m-°C
@Temperature 20.0 - 900 °C
 15.3 µm/m-°C
@Temperature 20.0 - 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.12 %
Chromium, Cr 5.0 %
Cobalt, Co 2.5 %
Iron, Fe 6.0 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo 24 %
Nickel, Ni 63 %
Silicon, Si <= 1.0 %
Vanadium, V <= 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reade Advanced Materials Wood's Metal Alloy (Sn + Pb + Bi + Cd)
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 625/ Alloy 718 12.7 mm plate weldments
California Fine Wire Alloy 486 Precious Metal Alloy
California Fine Wire Alloy 20-245 Precious Metal Alloy

NHAWAX / 17017

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.