MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot CAB-O-SIL® S-17D Fumed Silica
Categories: Other Engineering Material

Material Notes: Product highlights: CAB-O-SIL S-17D fumed silica is Cabot’s highest surface area fumed silica available. It imparts the highest reinforcement to silicone rubbers among Cabot fumed silica products. The bulk density of CAB-O-SIL S-17D fumed silica has been mechanically increased to promote faster incorporation and ease of handling. All untreated fumed silicas are characterized by:
  • High purity
  • Aggregated structure
  • Submicron particle size
  • Hydrophilic surface
Key applications: CAB-O-SIL S-17D fumed silica is suitable for use in the reinforcement of liquid silicone rubbed (LSR). It imparts the greatest increase in hardness, tensile strength and elongation at break out of all Cabot fumed silicas. For clear LSR applications, very well dispersed CAB-O-SIL S-17D fumed silica can provide excellent transparency. Because of the hydrophilic surface of untreated fumed silicas, further modification of the silica surface is necessary to prevent crepe hardening. Use of a densed, higher bulk density silica such as our CAB-O-SIL S-17D product requires very high shear dispersion equipment to achieve adequate dispersion of the silica. The higher bulk density of CAB-O-SIL S-17D fumed silica facilitates faster wet-in or incorporation into viscous polymer systems.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT093 / 315828

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.