MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Redwood Plastics TIVAR® CERAMP® UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: The ultimate material for high load, high speed and severe sliding abrasion applications. Composed of virgin polymer and premium additives, Redco™ Tivar® Ceram P® is a shatter-resistant alternative to ceramics, reducing wear and machine maintenance downtime.

Standard Color: Blue, White & Black

Fusion welded Redco™ UHMW sheets are available to eliminate lifting; up to 144” x 1200”.

Typical Applications: Belt skirting, chute liners, conveying components, bearings, belt guides, chain guides, curves, guide rails, wear strip, dead plates, diverter bars, guide rollers, hitch plates, hopper liners, liners for gravity flow applications, roller covers, transfer plates, under belt wear strips, belt scrapers, bunker liners, chain conveyor flights, chute liners, conveyor skirting, cyclones, drag chain conveyor liners, dragline buckets, dust collection hopper liners, front end loader bucket liners, hopper liners, off-road truck beds, truck bed lining for asphalt hauling, pugmill paddles, railcar liners, reclaimer buckets, screw conveyor liners, self-unloading ships, silo liners, slider beds, storage bin liners surge bin liners, transfer chute liners, under chain guides, vibrating bin, dischargers, vibratory feeder liners, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.964 g/cc0.0348 lb/in³ASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ASTM D 2240
Tensile Strength at Break 26.2 MPa3800 psiASTM D638
Tensile Strength, Yield 19.3 MPa2800 psiASTM D638
Elongation at Break 300 %300 %ASTM D 638
Tensile Modulus 0.90301 GPa130.97 ksiASTM D638
1% Secant Modulus 689.01 MPa99933 psiASTM D790B
Izod Impact, Notched NBNBASTM D256A
Tensile Impact Strength 1570 kJ/m²750 ft-lb/in²ASTM D1822
Coefficient of Friction, Dynamic 0.120.12(DRY vs. STEEL)
Coefficient of Friction, Static 0.180.18(DRY vs. STEEL)
Abrasion 8.08.0Sand Slurry, 1018 steel=100
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D 257
Surface Resistance 1.00e+17 ohm1.00e+17 ohmASTM D 257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C
@Temperature -30.0 - 60.0 °C
8.89 µin/in-°F
@Temperature -22.0 - 140 °F
ASTM D-2240
Maximum Service Temperature, Air 104 °C220 °FConstant
 116 °C240 °FIntermittent
 
Descriptive Properties
FDA ()NO
Sand on Wheel85 mg weight lossASTM G-64

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW016 / 296582

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.