MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Fibre Glast 1101 High-Strength General Purpose Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description:
#1101 is a light grayish-tan two part epoxy adhesive that was developed especially for difficult bonding problems involving similar or dissimilar materials. #1101 provides excellent adhesion to a wide variety of materials such as aluminum, steel, brass, concrete, brick, glass, stone, ceramics, tile, and wood. #1101 has very good handling characteristics. The mix ratio of 1 to 1 by weight or volume allows for easy measuring. It has a creamy, smooth viscosity. It is very easy to mix, and has good thixotropy for application to contoured or vertical surfaces without sag or runoff. #1101 cures relatively quickly, developing sufficient "green strength" to allow bonded items to be removed from the holding fixtures and handled within a few hours. The cured material has excellent strength as well as good resistance to weak acids, moisture and weather.

Applications
#1101 is an excellent adhesive for all types of bonding applications. It is very versatile, and can bond a wide variety of materials, so it becomes an effective tool in general shop situations. Often #1101 will outperform other supposed high performance materials, and give handling advantages as well. It has been successfully used for many years in a variety of general bonding uses as well as numerous production applications.

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D1475
Water Absorption <= 0.20 %<= 0.20 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090Cured; ASTM D2240
Tensile Strength at Break 49.6 MPa7200 psiCast bar; ASTM D638
Elongation at Break 6.0 %6.0 %ASTM D412
Compressive Yield Strength 98.6 MPa14300 psiASTM D695
Adhesive Bond Strength 24.0 MPa3480 psiLap Shear; Aluminum to Aluminum; ASTM D1002
 
Processing PropertiesMetricEnglishComments
Cure Time 180 - 240 min3.00 - 4.00 hourHandling strength in 3 to 4 hrs.
 45.0 - 60.0 min
@Temperature 60.0 °C
0.750 - 1.00 hour
@Temperature 140 °F
Full cure in 45 to 60 mins at 140°F.
 360 - 480 min
@Temperature 25.0 °C
6.00 - 8.00 hour
@Temperature 77.0 °F
Full Cure
Gel Time 20.0 - 30.0 min20.0 - 30.0 minValue for 1 lbm; ASTM D2471
 
Descriptive Properties
Mix Ratio1:1Resin:Hardener by Volume
 100:100Resin:Hardener by Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek WCB UNS J13345 Cast Alloy Steel

PFIBRE24 / 38293

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.