MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nevicolor NEVIFOOD PA6 G30 NATURALE Nylon 6, 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: Polyamide 6 reinforced with 30% glass fibre; suitable for food contact applications (Reg. EU 10/2011 and FDA)

Information provided by Nevicolor

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Moisture Absorption 2.00 %2.00 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/in115mm x 50mm x 3mm
Linear Mold Shrinkage, Transverse 0.0050 - 0.010 cm/cm0.0050 - 0.010 in/in115mm x 50mm x 3mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 185 MPa26800 psiISO 527-1/2
Elongation at Break 4.0 %4.0 %ISO 527-1/2
Modulus of Elasticity 10.0 GPa1450 ksi1 mm/min; ISO 527-1/2
Flexural Strength 250 MPa36300 psi2 mm/min; ISO 178
Flexural Modulus 8.50 GPa1230 ksiElastic; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 80.0 kJ/m²38.1 ft-lb/in²ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °F120°C/h; ISO 75/Ae
Vicat Softening Point 205 °C
@Load 5.10 kg
401 °F
@Load 11.2 lb
50°C/h; ISO 306/B
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNEVI053 / 267397

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.