MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

UBE UMERIT® UMERIT® 2515HF Film Superpolyethylene (Metallocene L-LDPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Additives: Antiblocking agent, Antioxidant. Features: Stiffness, Impact resistance, Excellent in blown film molding.

Applications: Film, Sheet, Heavy duty packing, Fertilizer bag. Property data reported for compression-molded sheets.

Information provided by UBE Industries, LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourF50; ASTM D1693
Melt Flow 0.90 g/10 min0.90 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ASTM D2240
Tensile Strength 36.0 MPa5220 psiASTM D638
Elongation at Break 715 %715 %ASTM D638
Flexural Modulus 0.370 GPa53.7 ksiASTM D790
Izod Impact Resistance NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 121 °C250 °FUBE method
Vicat Softening Point 112 °C234 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUBD9908 / 287371

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.