MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Johnson Matthey Soft Solder Flux No. 3S™ Flux Paste
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Soft Solder Flux No.3S™ Flux Paste is a predominantly designed for industrial soldering applications. It is recommended for use on all common engineering materials except aluminum. It is particularly suitable for use on carbon steel and stainless steel as well as being effective on copper and copper alloys such as brass.

Soft Solder Flux No.3S™ Flux Paste has an active or working range which goes up to 350°C. It can therefore be used with tin-copper solders and tin-silver solders. It is also suitable for use with specialized high temperature solders.

Soft Solder Flux No.3S™ Flux Paste is a semi-fluid light grey colored flux paste that can be readily applied by brushing onto components prior to heating.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 180 - 350 °C356 - 662 °F
Solidus 180 °C356 °F
Liquidus 350 °C662 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
In95-Bi5 Indium-Bismuth Solder
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
Nihon Superior LF-C2 Lead-Free Solder Alloy
In90-Ag10 Indium-Silver Solder

NJMMJ9784 / 186185

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.