MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Huber Onyx Elite® 431 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Onyx Elite® 431 initiates a new standard for alumina trihydrate fillers. Onyx Elite® 431 is a color controlled high-purity, organic-free Alumina Trihydrate specifically designed to provide the translucency, depth of pattern and soft white color that are so important to the cast polymer industry. Onyx Elite 431 is a high brightness product exhibiting a unique particle size distribution that provides the best combination of viscosity and air release for cast polymer. A closely controlled coarse fraction top size with a large fine fraction yields rapid dispersion in resin, excellent mold flow and wet-out characteristics, resulting in minimal porosity, even pigmentation, and excellent filler reinforcement throughout the molded part. Onyx Elite 431 is a low surface area, medium particle size flame retardant and smoke suppressant Alumina. A complete range of surface modifications is available to aid in processing and enhance physical properties.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.42 g/cc
Bulk Density 0.780 g/ccloose
 1.35 g/ccpacked
Moisture Absorption 0.300 %
@Temperature 105 °C
Free
Particle Size 8.0 µmMedian Particle Diameter
 <= 10 µm63 percent
Particle Mesh Size 100 Mesh0% on
 200 Mesh0.01% on
 325 Mesh1.0% on
 325 Mesh99% through
Specific Surface Area 2.0 m²/gBET
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 0.0040 %
Loss on Ignition(%) 34.6 %
@Temperature 1000 °C
Na2O 0.020 %soluble
 0.20 %total
SiO2 0.0080 %
 
Descriptive Properties
Al(OH)3 (%)99.6
Color90 L
Functionality: Optical effectsHigh Brightness / Transparency
Market/Application: ThermosetsSolid Surface/Cast Polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EHUBER762 / 300868

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.