MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kaltun STONETUN QUARTZ Q.-1200+500 for Stone Composites
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: STONETUN quartz is used in composite stone production and they increase the aesthetic appearance and functional performance of the composite stone. All STONETUN products are produced in mines belonging to Kaltun Madencilik A.S. and located in Çine-Milas region.

Information provided by KALTUN MINING

Key Words: Product Code: KKK.10.G.1205
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.65 g/cc0.0957 lb/in³
Moisture Absorption 0.200 %0.200 %
Loss On Ignition 0.10 %0.10 %
Particle Size 500 µm500 µm2% Screening (wet/dry)
 >= 500 µm>= 500 µm98% Screening (wet/dry)
 >= 1200 µm>= 1200 µm1% Screening (wet/dry)
 >= 1600 µm>= 1600 µm0% Screening (wet/dry)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 7.07.0
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.90 %0.90 %
CaO 0.040 %0.040 %
Fe2O3 0.020 %0.020 %
K2O 0.040 %0.040 %
MgO 0.030 %0.030 %
Na2O 0.27 %0.27 %
SiO2 98.6 %98.6 %
 
Descriptive Properties
Color1.25a; Spectrophotometer D65/10°
 3.6b; Spectrophotometer D65/10°
 82.5L; Spectrophotometer D65/10°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKALT858 / 318156

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.