Silicone rubber with high permittivity and addition curing two-component compound for manufacturing of extruded articles Special features: The material was especially designed for the production of devices in the Cable Accessories field. Application: Refractive Field Control Application: Production of Field Control Elements for Cable Accessories. Information provided by Wacker Chemie AG. |