MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Potters Industries Q-Cel® 7040S Hollow Engineered Glass Microspheres
Categories: Ceramic; Glass; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths meet specific functional and end-use application requirements such as reducing density or cost, or improving stiffness or workability. They are compatible with polyesters, epoxies, phenolic resins, urethanes, plastisols, thermoplastics, latex, concrete and other building materials, as well as emulsion- and water-gel explosives. They are available uncoated, or coated with specially-formulated coupling agents (CP01, CP03) to maximize interfacial bonding between the microspheres and the resin matrix.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.260 g/cc0.00937 lb/in³
Density 0.400 g/cc0.0145 lb/in³Effective Density as measured by liquid displacement
Particle Size 5.0 - 100 µm5.0 - 100 µm
 54 µm54 µmMean
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength <= 13.8 MPa<= 2000 psiWorking pressure
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) <= 0.50 %
@Temperature 121 °C,
Time 601 sec
<= 0.50 %
@Temperature 250 °F,
Time 0.167 hour
 
Descriptive Properties
Alkalinity< 0.5 meq/gASTM D3100
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CPOT9948 / 161938

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.