WESTLAKE low-density polyethylene EM1870 is used for injection molding applications. It has excellent stress crack resistance for lids.Application/Uses- Flexible medical
- Lids
- Medical
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical |
Excellent stress crack resistance |