MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Acclaim® 4200 Polyol
Categories: Polymer; Thermoset

Material Notes: Characterization: Acclaim 4200 polyol is a 4,000-molecular-weight diol based on propylene oxide.

Properties / Applications: Acclaim 4200 polyol is a high-performance, low-monol polyether that is prepared with Covestro's proprietary IMPACT™ technology, using a patented organo-metallic propoxylation catalyst. The terminal end-groups are predominantly secondary hydroxyls and have a relatively low reactivity. This polyol is acidified with a low level of phosphoric acid, making it suitable for use in isocyanate-terminated prepolymers. Acclaim 4200 polyol is used in polyurethane and other applications, including cast elastomers, sealants, epoxy flexibilizers, defoamers, lubricants, crude oil de-emulsifiers and plasticizers. Acclaim 4200 polyol is a complementary product to Acclaim 6300 polyol, an ultra-low monol triol with the same equivalent weight. Overall polyol functionality can easily be varied by blending these two polyols. This polyol contains extremely low levels of monol. In some polyurethane systems, formulation changes, such as reducing the crosslinking level or changing the hard-segment content, may be necessary to maximize the benefits of using Acclaim polyols. As with any product, use of Acclaim 4200 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/cc
 0.950 g/cc
@Temperature 90.0 °C
 0.980 g/cc
@Temperature 50.0 °C
 1.02 g/cc
@Temperature 0.000 °C
Bulk Density 62.8 lb/ft³
Viscosity 980 cP
 100 cP
@Temperature 80.0 °C
Storage Temperature 15.0 - 60.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.020[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Flash Point 213 °CPMCC
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.030 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<50 Pt-Co
Hydroxyl number26.5-29.5 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Acclaim® 8200 Polyol
Covestro Baygal® 90 IK 51 Polyurethane
Covestro Baygal® 90 IK 20 Polyurethane
Covestro Acclaim® 2200 Polyol

PCOVEST0005 / 201788

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.