MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Barlog Plastics KEBAFLEX P D55.3 HR TPC-ET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: KEBAFLEX / P D55.3 HR is a polyester elastomer with a Shore hardness of 55 D. The material is free of plasticizers and is characterized by its very good flexibility and impact strength, even at low temperatures. Compared to the standard grade KEBAFLEX / P D55.1, KEBAFLEX / P D55.3 HR exhibits improved recovery behavior and a higher melting temperature.

Properties: flexible, good gliding properties, good recovery behavior, High wear resistance, semi-crystalline

Typical areas of application: Axle collars, Airbag covers, Sealing elements, Spring elements, Sliding elements, Hoses, Vibration damper, Sports & Leisure Articles, shockproof housing, Gears, Timing belt

Industries: Automotive, Railroad industry, Electrical and electronics industry, Household appliances, Industry, Agriculture, Food processing industry, Mechanical Engineering, Medical Technology, Furniture industry, Sports & Recreation

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183-1
Linear Mold Shrinkage, Flow 0.0120 cm/cm0.0120 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0120 cm/cm0.0120 in/inISO 294-4
Melt Flow 15.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50.050.0DIN ISO 7619-1
Tensile Strength, Yield 13.0 MPa1890 psiISO 527-1
 10.0 MPa
@Strain 10.0 %
1450 psi
@Strain 10.0 %
DIN EN ISO 527-1
Elongation at Break 500 %500 %ISO 527-1
Elongation at Yield 40.0 %40.0 %ISO 527-1
50% Modulus 13.0 MPa
@Strain 50.0 %
13.0 MPa
@Strain 50.0 %
DIN EN ISO 527-1
100% Modulus 13.0 MPa
@Strain 100 %
1890 psi
@Strain 100 %
DIN EN ISO 527-1
300% Modulus 17.0 MPa
@Strain 300 %
2470 psi
@Strain 300 %
DIN EN ISO 527-1
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 10.0 J/cm²47.6 ft-lb/in²ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 180 µm/m-°C100 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C100 µin/in-°FISO 11359-1/-2
Melting Point 200 °C392 °FISO 11357-1/-3
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 245 °C446 - 473 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hour
Moisture Content <= 0.0200 %<= 0.0200 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO511 / 326585

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.