MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Solef® 5120 PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.

Applications: Batteries; Binder

Features: Good Adhesion; Medium Viscosity

Intrinsic Viscosity: 0.15 - 0.25 l/g

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 - 1.78 g/cc0.0632 - 0.0643 lb/in³ISO 1183
Water Absorption <= 0.20 %
@Time 86400 sec
<= 0.20 %
@Time 24.0 hour
ASTM D570
Melt Flow <= 3.0 g/10 min
@Load 21.6 kg,
Temperature 230 °C
<= 3.0 g/10 min
@Load 47.6 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 1.00 - 1.50 GPa145 - 218 ksi1.0 mm/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 38.0 - 48.0 J/g16.3 - 20.6 BTU/lbASTM D3418
Melting Point 160 - 168 °C320 - 334 °F
Crystallization Temperature 124 - 130 °C255 - 266 °FPeak; ASTM D3418
Glass Transition Temp, Tg -40.0 °C-40.0 °FDSC
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4476 / 280276

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.