MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Spectar™ Renew 14471-15 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Spectar™ Renew 14471-15 copolyester is a sparkling, clear plastic material that is increasingly popular for protective barriers used to limit the spread of viruses like COVID-19, including sneeze guards. For these applications, Spectar™ Renew 14471-15 is a proven alternative to polycarbonate and acrylic. Eastman Spectar™ Renew 14471-15 copolyester is BPA free, environmentally friendly, fire and shatter resistant, long lasting, and resistant to common commercial cleaning agents. It can be found in a variety of end applications around the world, like point-of-purchase displays; separation barriers; signs; light fixtures at retailers, schools, hospitals, and office buildings; and sneeze guards. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.GREENGUARD Certification recognizes Eastman for manufacturing products with low chemical and particle emissions for better indoor environments. For more information about GEI and to obtain printable certificates for Eastman copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the “Manufacturer” category and click search to display a list of our products. This product is certified to NSF/ANSI Standard 51 for Food Equipment Materials. This product has received a Platinum level Material Health Certificate from the Cradle to Cradle Products Innovation Institute. A Material Health Certificate is awarded to products that meet the Material Health requirements of the multi-attribute Cradle to Cradle Certified™ Product Standard. The Cradle to Cradle Products Innovation Institute is a nonprofit organization that administers the publicly available Cradle to Cradle Certified™ Product Standard, which provides designers and manufacturers with criteria and requirements for continually improving product materials and manufacturing processes. The Material Health Certificate provides manufacturers with a trusted way to communicate their efforts to identify and replace chemicals of concern in their products. For more information about Cradle to Cradle certification and to obtain printable certificates for Eastman copolyesters, visit www.c2ccertified.org. Search for Eastman Chemical Company in the Material Health Certificate Registry. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Building materials
  • Displays/in-store fixtures
  • Indoor signs
  • Lighting
  • Point-of-purchase
  • Shelving solutions-retail
  • Skylights
  • Thermoformed sheet
  • Visual merchandising
  • Walls
Key Attributes
  • Acrylic alternative (PMMA alternative)
  • BPA free
  • Easily formed and shaped
  • Free of materials of concern
  • Glasslike clarity
  • Naturally smooth edges
  • Passes NFP 286 flammability test
  • Polycarbonate alternative (PC alternative)
  • Resilient to most commercial disinfectants and cleaning agents
  • Scratches can be easily removed with a common heat gun
  • Shatter resistant

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D1505
Water Absorption 0.200 %
@Time 86400 sec
0.200 %
@Time 24.0 hour
immersion; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Tensile Strength at Break 26.0 MPa3770 psiISO 527
 26.0 MPa3770 psiASTM D638
Tensile Strength, Yield 53.0 MPa7690 psiISO 527
 53.0 MPa7690 psiASTM D638
Elongation at Break 40.0 %40.0 %ISO 527
 50.0 %50.0 %ASTM D638
Elongation at Yield 4.70 %4.70 %ISO 527
 4.80 %4.80 %ASTM D638
Tensile Modulus 2.20 GPa319 ksiISO 527
 2.20 GPa319 ksiASTM D638
Flexural Strength 69.0 MPa10000 psiISO 178
Flexural Modulus 2.10 GPa305 ksiISO 178
Izod Impact, Notched  0.390 J/cm
@Temperature -30.0 °C
0.731 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 0.660 J/cm
@Temperature 0.000 °C
1.24 ft-lb/in
@Temperature 32.0 °F
ASTM D256
 0.880 J/cm
@Temperature 23.0 °C
1.65 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ASTM D4812
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO)  4.40 kJ/m²
@Temperature -30.0 °C
2.09 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 6.10 kJ/m²
@Temperature 0.000 °C
2.90 ft-lb/in²
@Temperature 32.0 °F
ISO 180
 11.5 kJ/m²
@Temperature 23.0 °C
5.47 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179
 NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  0.440 J/cm²
@Temperature 0.000 °C
2.09 ft-lb/in²
@Temperature 32.0 °F
ISO 179
 0.610 J/cm²
@Temperature -40.0 °C
2.90 ft-lb/in²
@Temperature -40.0 °F
ISO 179
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Puncture Energy  33.0 J
@Temperature 23.0 °C
24.3 ft-lb
@Temperature 73.4 °F
@ Max. Load; ASTM D3763
 40.0 J
@Temperature 0.000 °C
29.5 ft-lb
@Temperature 32.0 °F
@ Max. Load; ASTM D3763
 42.0 J
@Temperature -10.0 °C
31.0 ft-lb
@Temperature 14.0 °F
@ Max. Load; ASTM D3763
 43.0 J
@Temperature -20.0 °C
31.7 ft-lb
@Temperature -4.00 °F
@ Max. Load; ASTM D3763
 47.0 J
@Temperature -30.0 °C
34.7 ft-lb
@Temperature -22.0 °F
@ Max. Load; ASTM D3763
 59.0 J
@Temperature 23.0 °C
43.5 ft-lb
@Temperature 73.4 °F
@ Max. Load; ISO 6603-2
 61.0 J
@Temperature 0.000 °C
45.0 ft-lb
@Temperature 32.0 °F
@ Max. Load; ISO 6603-2
 70.0 J
@Temperature -10.0 °C
51.6 ft-lb
@Temperature 14.0 °F
@ Max. Load; ISO 6603-2
 73.0 J
@Temperature -20.0 °C
53.8 ft-lb
@Temperature -4.00 °F
@ Max. Load; ISO 6603-2
 74.0 J
@Temperature -30.0 °C
54.6 ft-lb
@Temperature -22.0 °F
@ Max. Load; ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+16 ohm1.00e+16 ohmASTM D257
Dielectric Constant  2.40
@Frequency 1.00e+6 Hz
2.40
@Frequency 1.00e+6 Hz
ASTM D150
 2.60
@Frequency 1000 Hz
2.60
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.1 kV/mm409 kV/inShort Time, 500 V/sec rate-of-rise; ASTM D149
Dissipation Factor  0.00500
@Frequency 1000 Hz
0.00500
@Frequency 1000 Hz
ASTM D150
 0.0200
@Frequency 1.00e+6 Hz
0.0200
@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 158 sec158 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C162 °FISO 75
 74.0 °C165 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FISO 75
 70.0 °C158 °FASTM D648
Vicat Softening Point 83.0 °C181 °FASTM D1525
 78.0 °C
@Load 5.00 kg
172 °F
@Load 11.0 lb
ISO 306
 83.0 °C
@Load 1.00 kg
181 °F
@Load 2.20 lb
ISO 306
Flammability, UL94 V-2V-2
Oxygen Index 26.0 %26.0 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.571.57ASTM D542
Haze <= 1.00 %<= 1.00 %ASTM D1003
Gloss 159 %159 %60°; ASTM D523
Yellow Index <= 1.50 %<= 1.50 %CIELAB, Illuminant D6500, 10° Observer; ASTM D1925
Transmission, Visible 89.0 %89.0 %Regular; ASTM D1003
 91.0 %91.0 %Total; ASTM D1003
 
Compliance PropertiesMetricEnglishComments
NSF YesYesSee notes for details
 
Descriptive Properties
Color<1b*, CIELAB, Illuminant D6500, 10° Observer; ASTM E308

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4147 / 323770

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.