MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKROSPERSE® E-29072 Dispersion
Categories: Other Engineering Material

Material Notes: Product Description: Akrosperse E-29072 is a dispersion of 90% active antimony oxide treated with a liquid chlorinated paraffin. The physical form is a reduced dust, free-flowing powder. The 90% dispersion of antimony oxide is a proven means of upgrading plant safety, efficiency, quality and raw material control. This physical form helps minimize irritating dust, as well as other potential hazards in handling antimony powders in the plant and is easily incorporated into rubber and plastic compounds.

Applications: Akrosperse E-29072 is an excellent flame retarder for elastomeric and plastic compounds with a typical loading range of 5% - 30%. In combination with additional halogenated donors, Akrosperse E-29072 reacts synergistically to increase the flame resistance of non-halogenated compounds. Halogenated compounds may not require addition halogen donors.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 4.00 - 4.10 g/cc
 
Descriptive Properties
Appearancedamp powder off-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH249 / 315167

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.