MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC SABIC® LDPE HP0323NN PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: HP0323NN is a Low Density Polyethylene grade suitable for producing heavy-duty films. It gives outstanding toughness and optical properties in the film. It contains no slip, no antiblock and no antioxidant additives.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D1505
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 12.0 MPaProperties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D882
Film Tensile Strength at Yield, TD 12.0 MPaProperties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D882
Film Elongation at Break, MD 235 %Properties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D882
Film Elongation at Break, TD 570 %Properties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D882
Elmendorf Tear Strength, MD 2.40 g/micronProperties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D1922
Elmendorf Tear Strength, TD 3.00 g/micronProperties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D1922
Dart Drop 2.00 g/micronProperties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D1709
Film Tensile Strength at Break, MD 32.0 MPaProperties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D882
Film Tensile Strength at Break, TD 30.0 MPaProperties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D882
1% Secant Modulus, MD 200 MPaProperties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D882
1% Secant Modulus, TD 260 MPaProperties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 95.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 15 %
@Thickness 0.0500 mm
2.5 BUR using 100% HP0323NN.; ASTM D1003
Gloss 38 %45°; Properties have been measured by producing 50 µm film with 2.5 BUR using 100% HP0323NN.; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10988 / 244455

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.